Two BMC impact values are not automatically comparable, even when the material descriptions look similar. A purchasing team should confirm how the specimens were produced and tested before making a ranking or writing a finished-part requirement.
Record the specimen origin and geometry
Distinguish test bars molded separately from samples removed from a finished part. For a cut specimen, identify location and direction on a marked drawing. Record specimen geometry and whether the notch is required by the specified test method; do not mix notched and unnotched results.
Identify the actual method and result basis
ASTM D256 describes Izod pendulum methods for plastics, not a universal impact rating. Ask for the exact method designation and edition, conditioning, report units and individual results. Record the observed break classification when the method calls for it. A result from a different test configuration is not a drop-in replacement.
Use a separate test for assembled risk
If the practical concern is damage at a rib, corner or mounting point, use material tests to screen options and agree a finished-part test for the assembly condition. Define how the part is supported, where impact is applied and what visible or functional damage constitutes failure.
What to include in the RFQ
- Method, edition, specimen dimensions and conditioning
- Specimen source, location, orientation and notch details
- Separate finished-part test and acceptance requirements if needed
When environmental exposure is part of the requirement, define what an exposure test must represent before using the reported results.
Technical reference: ASTM D256 Izod pendulum impact resistance.